AS 1330:2019 Metallic materials - Drop weight tear test for steels
(edit with the Customer Reassurance module)
(edit with the Customer Reassurance module)
(edit with the Customer Reassurance module)
This Standard specifies the method for conducting a drop weight tear test (DWTT) for carbon steel, low alloy steel, and similar materials. In particular, it applies to testing line-pipe, and strip or plate intended for line-pipe of 150 mm in diameter or greater but excludes the testing of weld metal. Where thickness is greater than 19 mm, an alternative method is permitted.